Fiberglass Composites Manufacturing Processes Brief - TopicsExpress



          

Fiberglass Composites Manufacturing Processes Brief Introduction: There are two general divisions of composites manufacturing processes: open molding and closed molding. With open molding, the gel coat and laminate are exposed to the atmosphere during the fabrication process. In closed molding, the composite is processed in a two-sided mold set, or within a vacuum bag. There are a variety of processing methods within the open and closed molding categories: OPEN MOLDING Hand Lay-Up Spray-up Filament Winding CLOSED MOLDING Compression molding Pultrusion Reinforced Reaction Injection Molding (RRIM) Resin Transfer Molding (RTM) Vacuum Bag Molding Vacuum Infusion Processing Centrifugal Casting Continuous Lamination Selecting which manufacturing process to select depends on a number of factors including cost, materials, size, and most important volume. Below is what processes would be used depending on production amounts: Low Volume Production Hand Lay-up Vacuum Bag Molding Vacuum Infusion Processing Medium Volume Production Filament Winding Wet Lay-Up Compression Molding Resin Transfer Molding Centrifugal Casting High Volume Production Compression Molding Pultrusion Reinforced Reaction Injection Molding Continuous Lamination OPEN MOLDING The heart of the open molding process is saturating fiber reinforcement with resin, then using manual roll-out techniques to consolidate the laminate and remove entrapped air. A major factor in this operation is the transfer of resin from a drum or storage tank to the mold. The means used to transport the resin, in many cases, characterizes the specific process method. Hand Lay-Up Hand lay-up is an open molding method suitable for making a wide variety of composites products including: boats, tanks, bathware, housings, RV/truck/auto components, architectural products, and many other products ranging from very small to very large. Production volume per mold is low; however, it is feasible to produce substantial production quantities using multiple molds. Process Description - Gel coat is first applied to the mold using a spray gun for a high-quality surface. When the gel coat has cured sufficiently, roll stock fiberglass reinforcement is manually placed on the mold. The laminating resin is applied by pouring, brushing, spraying, or using a paint roller. FRP rollers, paint rollers, or squeegees are used to consolidate the laminate, thoroughly wetting the reinforcement, and removing entrapped air. Subsequent layers of fiberglass reinforcement are added to build laminate thickness. Low density core materials, such as end-grain balsa, foam, and honeycomb, are commonly used to stiffen the laminate to produce sandwich construction. Molds - Simple, single-cavity molds of fiberglass composites construction are generally used. Molds can range from very small to very large and are low cost in the spectrum of composites molds. Major Advantages - Simplest method offering low-cost tooling, simple processing, and a wide range of part sizes. Design changes are readily made. There is a minimum investment in equipment. With skilled operators, good production rates and consistent quality are obtainable. Spray-Up (Chopping) Spray-up or chopping is an open mold method similar to hand lay-up in its suitability for making boats, tanks, transportation components and tub/shower units in a large variety of shapes and sizes. A chopped laminate has good conformability and is sometimes faster than hand lay-up in molding complex shapes. In the spray-up process the operator controls thickness and consistency, therefore the process is more operator dependent than hand lay-up. Although production volume per mold is low, it is feasible to produce substantial production quantities using multiple molds. Process Description - As with hand lay-up, gel coat is first applied to the mold prior to spray-up of the substrate laminate. Continuous strand glass roving and catalyzed resin are fed through a chopper gun, which deposits the resin-saturated chop on the mold. The laminate is then rolled to thoroughly saturate the glass strands and compact the chop. Additional layers of chop laminate are added as required for thickness. Roll stock reinforcements, such as woven roving or knitted fabrics, can be used in conjunction with the chopped laminates. Core materials of the same variety as used in hand lay-up are easily incorporated. Molds - These are the same molds as in hand lay-up simple, single-cavity, molds of fiberglass composites construction. Molds can range from very small to very large and are low cost in the spectrum of composites molds. Major Advantages - Simple, low-cost tooling, simple processing; portable equipment permits on-site fabrication; virtually no part size limitations. The process may be automated. Filament Winding Filament winding is an automated open molding process that uses a rotating mandrel as the mold. The male mold configuration produces a finished inner surface and a laminate surface on the outside diameter of the product. Filament winding results in a high degree of fiber loading, which provides high tensile strengths in the manufacture of hollow, generally cylindrical products such as chemical and fuel storage tanks, pipes, stacks, pressure vessels, and rocket motor cases. Process Description - Continuous strand roving is fed through a resin bath and wound onto a rotating mandrel. The roving feed runs on a trolley that traverses the length of the mandrel. The filament is laid down in a predetermined geometric pattern to provide maximum strength in the directions required. When sufficient layers have been applied, the laminate is cured on the mandrel. The molded part is then stripped from the mandrel. Equipment is available for filament winding on a continuous basis and two axis winding for pressure cylinders. Filament winding can be combined with the chopping process and is known as the hoop chop process. Molds - Mandrels of suitable size and shape, made of steel or aluminum form the inner surface of the hollow part. Some mandrels are collapsible to facilitate part removal. Major Advantages - The process makes the high strength-to-weight ratio laminates and provides a high degree of control over uniformity and fiber orientation. The filament winding process can be used to make structures which are highly engineered and meet strict tolerances. Because filament winding is automated, the labor factor for filament winding is lower than other open molding processes. CLOSED MOLDING Compression Molding Compression molding is a high-volume, high-pressure method suitable for molding complex, fiberglass-reinforced plastic parts on a rapid cycle time. There are several types of compression molding including: sheet molding compound (SMC) which are, bulk molding compound (BMC), thick molding compound (TMC), and wet lay-up compression molding. Compression molding tooling consists of heated metal molds mounted in large presses. Process Description - The mold set is mounted in a hydraulic or mechanical molding press. The molds are heated to 2500 to 4000 F. A weighed charge of molding compound is placed in the open mold. The two halves of the mold are closed and pressure is applied. Depending on thickness, size, and shape of the part, curing cycles range from less than a minute to about five minutes. The mold is opened and the finished part is removed. Typical parts include: automobile components, appliance housings and structural components, furniture, electrical components, and business machine housings and parts. Molds - Tooling is usually machined steel or cast alloy molds that can be in either single or multiple-cavity configurations. Steel molds are hardened and sometimes chrome plated for enhanced durability. The molds are heated using steam, hot oil, or electricity. Side cores, provisions for inserts, and other refinements are often employed. Mold materials include cast of forged steel, cast iron, and cast aluminum. Matched metal molds can cost fifty times as much as an FRP open mold and tooling in the $50,000-$500,000 range is not uncommon. Major Advantages - Compression molding produces fast molding cycles and high part uniformity. The process can be automated. Good part design flexibility and features such as inserts, ribs, bosses, and attachments can be molded in. Good surface finishes are obtainable, contributing to lower part finishing cost. Subsequent trimming and machining operations are minimized in compression molding. Labor costs are low. Pultrusion Pultrusion is a continuous process for the manufacture of products having a constant cross section, such as rod stock, structural shapes, beams, channels, pipe, tubing, fishing rods, and golf club shafts. Pultrusion produces profiles with extremely high fiber loading, thus pultruded products have high structural properties. Process Description - Continuous strand fiberglass roving, mat, cloth, or surfacing veil is impregnated in a resin bath, then pulled (pul-trusion) through a steel die, by a powerful tractor mechanism. The steel die consolidates the saturated reinforcement, sets the shape of the stock, and controls the fiber/resin ratio. The die is heated to rapidly cure the resin. Many creels (balls) of roving are positioned on a rack, and a complex series of tensioning devices and roving guides direct the roving into the die. Molds - Hardened steel dies are machined and include a preform area to do the initial shaping of the resin-saturated roving. The dies include heating which can be electric or hot oil. The latest pultrusion technology uses direct injection dies, in which the resin is introduced inside the die, rather than through an external resin bath. Major Advantages - The process is a continuous operation that can be readily automated. It is adaptable to both simple and complex cross-sectional shapes. Very high strengths are possible due to the fiber loading and labor costs are low. Vacuum Bag Molding The mechanical properties of open-mold laminates can be improved with vacuum bagging. By reducing the pressure inside the vacuum bag, external atmospheric pressure exerts force on the bag. The pressure on the laminate removes entrapped air, excess resin, and compacts the laminate. A higher percentage of fiber reinforcement is the result. Additionally, vacuum bagging reduces styrene emissions. Vacuum bagging can be used with wet-lay laminates and prepreg advanced composites. In wet lay-up bagging the reinforcement is saturated using hand lay-up, then the vacuum bag is mounted on the mold and used to compact the laminate and remove air voids. In the case of pre-impreg advanced composites molding, the prepreg material is laid-up on the mold, the vacuum bag is mounted and the mold is heated or the mold is placed in an autoclave that applies both heat and external pressure, adding to the force of atmospheric pressure. The prepreg-vacuum bag-autoclave method is most often used to create advanced composites used in aircraft and military products. Process Description - In the simplest form of vacuum bagging, a flexible film (PVA, nylon, mylar, or polyethylene) is placed over the wet lay-up, the edges sealed, and a vacuum drawn. A more advanced form of vacuum bagging places a release film over the laminate, followed by a bleeder ply of fiberglass cloth, non-woven nylon, polyester cloth, or other material that absorbs excess resin from the laminate. A breather ply of a non-woven fabric is placed over the bleeder ply, and the vacuum bag is mounted over the entire assembly. Pulling a vacuum from within the bag uses atmospheric pressure to eliminate voids and force excess resin from the laminate. The addition of pressure further results in high fiber concentration and provides better adhesion between layers of sandwich construction. When laying non-contoured sheets of PVC foam or balsa into a female mold, vacuum bagging is the technique of choice to ensure proper secondary bonding of the core to the outer laminate. Molds - Molds are similar to those used for conventional open-mold processes. Major Advantages - Vacuum bag processing can produce laminates with a uniform degree of consolidation, while at the same time removing entrapped air, thus reducing the finished void content. Structures fabricated with traditional hand lay-up techniques can become resin rich and vacuum bagging can eliminate the problem. Additionally, complete fiber wet-out can be accomplished if the process is done correctly. Improved core-bonding is also possible with vacuum bag processing. Vacuum Infusion Processing Vacuum infusion is a variation of vacuum bagging where the resin is introduced into the mold after the vacuum has pulled the bag down and compacted the laminate. The method is defined as having lower than atmospheric pressure in the mold cavity. The reinforcement and core material are laid-up dry in the mold. This is done by hand and provides the opportunity to precisely position the reinforcement. When the resin is pulled into the mold the laminate is already compacted; therefore, there is no room for excess resin. Very high resin to glass ratios are possible with vacuum infusion and the mechanical properties of the laminate are superior. Vacuum infusion is suitable to mold very large structures and is considered a low volume molding process. Process Description - The mold may be gel coated in the traditional fashion. After the gel coat cures, the dry reinforcement is positioned in the mold. This includes all the plies of the laminate and core material if required. A perforated release film is placed over the dry reinforcement. Next a flow media consisting of a coarse mesh or a crinkle ply is positioned, and perforated tubing is positioned as a manifold to distribute resin across the laminate. The vacuum bag is then positioned and sealed at the mold perimeter. A tube is connected between the vacuum bag and the resin container. A vacuum is applied to consolidate the laminate and the resin is pulled into the mold. Molds - Molds are similar to those used for conventional open-mold processes. Major Advantages - Vacuum infusion can produce laminates with a uniform degree of consolidation, producing high strength, lightweight structures. This process uses the same low cost tooling as open molding and requires minimal equipment. Very large structures can be fabricated using this method. Vacuum infusion offers a substantial emissions reduction compared to either open molding or wet lay-up vacuum bagging. Resin Transfer Molding Resin transfer molding is an intermediate volume molding process for producing composites. The RTM process is to inject resin under pressure into a mold cavity. RTM can use a wide variety of tooling, ranging from low cost composite molds to temperature controlled metal tooling. This process can be automated and is capable of producing rapid cycle times. Vacuum assist can be used to enhance resin flow in the mold cavity. Process Description - The mold set is gel coated conventionally, if required. The reinforcement (and core material) is positioned in the mold and the mold is closed and clamped. The resin is injected under pressure, using mix/meter injection equipment, and the part is cured in the mold. The reinforcement can be either a preform or pattern cut roll stock material. Preforms are reinforcement that is pre-formed in a separate process and can be quickly positioned in the mold. RTM can be done at room temperature; however, heated molds are required to achieve fast cycle times and product consistency. Clamping can be accomplished with perimeter clamping or press clamping. Molds - RTM can utilize either hard or soft tooling, depending upon the expected duration of the run. Soft tooling would be either polyester or epoxy molds, while hard tooling may consist of cast machined aluminum, electroformed nickel shell, or machined steel molds. RTM can take advantage of the broadest range of tooling of any composites process. Tooling can range from very low cost to very high cost, long life molds. Major Advantages - This closed molding process produces parts with two finished surfaces. By laying up reinforcement material dry inside the mold, any combination of materials and orientation can be used, including 3-D reinforcements. Part thickness is determined by the tool cavity. Fast cycle times can be achieved in temperature controlled tooling and the process can range from simple to highly automated.
Posted on: Wed, 12 Mar 2014 07:27:10 +0000

Trending Topics



px;"> Con amore e solo per amore soffrirò per te, questo cuore tu lhai
Breaking news: Anti-war activists enter military base 2
Greetings!I trust we are all doing fine.Just a quick one

Recently Viewed Topics




© 2015